So question has come up on proper temperature for salt bath annealing. Consensus seems to be 500-550C which is around the 1000F mark and a duration from around 4-7 seconds. Seeing some info for other annealing methods that are shooting for 750F. That’s like a 250F difference! Does anyone have information on why salt bath method is using that temp? Does doing so over anneal the brass?