Thank you Frank for that clarification.B.S. !!!!!!!!!!!!!!!!!
That was a pretty offensive statement you made and not knowing any of the details.
The ringing of the chamber with the hybrid cases cannot be stopped running the pressures at 80k psi so far from what I understand.
The ring will show up at the junction where the steel case head meets the brass body of the case.
Run the round at 65k and it behaves like everything else. Run it at 80k and things are going to change. No way around it.
Even Sig has told us our BB material stands up better to the abuse of 80k psi vs standard 416R and we have made them a ton of barrels for R&D as well as we make them a lot of ammunition test barrels. Both accuracy and pressure and velocity.
On production guns they are adding coatings and metal treatments to help with the ringing of the chambers to prolong service life.
I just love it when people say things and they have no clue as to what is going on!
Later, Frank
Bartlein Barrels
Thanks for responding. Not sure if I misunderstood it or not but it came across as it was bad material from us. That's how it looked.Thank you Frank for that clarification.
BTW, I think you simply misunderstood what I said.
What issue(s) does that ringing present when if forms?
Difficulty chambering cartridges? More pressure? Damage to cases, shortening case life?
Thanks for the info and the dialogue. It's much appreciated.Thanks for responding. Not sure if I misunderstood it or not but it came across as it was bad material from us. That's how it looked.
What issues does it bring up the ring/groove that is made in the chamber.
I do know that even before the ring starts at 80k psi bolt lift is very hard. To the point that you have to beat it open.
Around 500ish rounds the ring in the chamber from what I've seen is approx. .001" deep. Around 700ish rounds the ring/groove is around .002" deep. I've seen it and heard it from a three different places now. With measurements and pictures to back it up. This is in standard good quality 416R material. I do believe CM material reacts the same way. Extraction gets even more difficult as the ring/groove becomes more pronounced. I've been told by the same makers/ammo maker/testers that the 400modBB material stands up better but does not make it go away. That's why they are coating/metal treating the steel and chambers on the production guns to extend the barrel wear/life of the chamber to help prevent it from being a real problem.
The heat generated at 80k psi is much greater also. Also at 80k psi when you run the barrel a shorter length you can expect it to possibly cause accuracy issues. Same thing is seen with 338 Lapua. Even though the 338 Lapua isn't at 80k psi when you run the barrel length shorter (down to 20" finish vs a 24" or 26" or 27" etc...) there is so much pressure behind the heel of the bullet when it leaves the muzzle it causes the bullet to be tipping up more at the heel and it takes longer for the bullet to possibly recover which can effect the accuracy.
^^^^ what Walt said above! Walt can correct me if I'm wrong to what I type below.The ring is formed from the steel head not springing back like brass does. I played with it a little and decided for a competition gun the barrel life was just going to be too short to fool with it. The Remington actions used for testing have held up well except for the beating they take opening and extracting the rounds.
Welcome!Thanks for the info and the dialogue. It's much appreciated.
I think you're right on about that extra pressure on the heel of a bullet causing a little more tipping that'll cause a longer time for it to stabilize. I hadn't given that aspect any thought before.
The ring is formed from the steel head not springing back like brass does. I played with it a little and decided for a competition gun the barrel life was just going to be too short to fool with it. The Remington actions used for testing have held up well except for the beating they take opening and extracting the rounds.
I do fully understand the different metal properties (as someone who's worked with various aircraft sheetmetals), where brass and steel react to pressure differently.^^^^ what Walt said above! Walt can correct me if I'm wrong to what I type below.
You have two dissimilar metals... brass case body and the steel case head. They will expand/react differently under pressure. I think that is the issue.
Yes I call it a ring. Call it a ridge, shoulder, lip etc...
. . . and if it's a powder that doesn't completely burn in those short barrels, that can exacerbate that too. . . huh?Welcome!
The pressure on the heel of the bullet leaving the muzzle in the shorter barrels has been proven. Again not just in this caliber but like 338 Lapua like I stated earlier. Again in the 338 Lapua shooting a 20" barrel length it's going to be harder to get that gun to shoot say sub .75moa. Most likely more in the range of .75 to 1moa but shoot a longer barrel like 24" or 27" and the same loads will shoot better or should I say more consistently smaller groups. Just the nature of the beast.
How short and where does it start to show it's ugly face or start to show possible issues. That I cannot answer exactly. Might be a case of... what is your accuracy requirement?
I know from going to a 16" barrel and getting a .8moa with no problem... but as they chopped off 1" off each time the accuracy deteriorated steadily. At 13" if I recall correctly.... it was tough to get it under 1.3moa or so.
Now how much better does a 20" or 24" shoot? That I can't tell you.
Leave your barrel a longer length from an accuracy point of view is going to do nothing but help.
Picture a ball peen hammer hitting a piece of steel. It leaves a dent. The steel head of the case is doing the same thing to the barrel at the higher pressures this cartridge is designed for. A little bit at a time until there is a groove that restricts extraction.I do fully understand the different metal properties (as someone who's worked with various aircraft sheetmetals), where brass and steel react to pressure differently.
I was a bit surprised when I resized one of these cases after firing it that the steel web area had so easily been sized down to the same dimension before being fired (no noticeable difference from a standard brass case). I was expecting it so spring back more where I could measure it. Maybe it did and it's just that my caliper just doesn't have the resolution to see it???
I'm very curious about the physics as to how that junction produces a grooved ring on the steel surface of a steel barrel. (I just have in insatiable curiosity about how things work, all things . . . which propelled me into precision reloading).
View attachment 1685900
. . . and if it's a powder that doesn't completely burn in those short barrels, that can exacerbate that too. . . huh?
Why not is because the military was/is after something new that meets their specifications. The military was after a new generation weapon system. It's like when the military went from the M1 Garand to the M14.So I found a couple of these cases in the dirt at the range and started looking into it. Looks like it's basically a 7-08 that runs a few fps faster. What's the point, is there really an advantage worth the extra cost/ complexity/risk? I mean I understand what Sig's motivation is but why not just rebarrel an AR10 to 7-08? Not trying to start an argument just curious.
So You really Have No Clue.So I found a couple of these cases in the dirt at the range and started looking into it. Looks like it's basically a 7-08 that runs a few fps faster. What's the point, is there really an advantage worth the extra cost/ complexity/risk? I mean I understand what Sig's motivation is but why not just rebarrel an AR10 to 7-08? Not trying to start an argument just curious.
It wasn't Sig's doing.So I found a couple of these cases in the dirt at the range and started looking into it. Looks like it's basically a 7-08 that runs a few fps faster. What's the point, is there really an advantage worth the extra cost/ complexity/risk? I mean I understand what Sig's motivation is but why not just rebarrel an AR10 to 7-08? Not trying to start an argument just curious.
A standard loaded 7mm-08 won't make the velocity spec given. So basically a new round needed to be developed.So I found a couple of these cases in the dirt at the range and started looking into it. Looks like it's basically a 7-08 that runs a few fps faster. What's the point, is there really an advantage worth the extra cost/ complexity/risk? I mean I understand what Sig's motivation is but why not just rebarrel an AR10 to 7-08? Not trying to start an argument just curious.