+1 to all of these methods; I use them all for different situations (clean dies between uses!)
My consistent method for brass I anneal, resize, and otherwise treat so often that each case has a name:. Imperial sizing wax on body with neck first dipped in graphite. IE graphite on neck; was on body and I don't touch the graphite with wax. Works great for making 6.5 Grendel from 7.62x39; and keeping my 30-06 happy.
I do believe your original question was bulk sizing / application. The alcohol and lanolin is what I use; dump in 1 gallon freezer bag; a few sprays (reuse bag); and then roll around on flat tray to dry. Works fine on turning machine gun brass into usable cases for 7.62 and 5.56. if only I had a faster way to remove the crimps.
-Mac
My consistent method for brass I anneal, resize, and otherwise treat so often that each case has a name:. Imperial sizing wax on body with neck first dipped in graphite. IE graphite on neck; was on body and I don't touch the graphite with wax. Works great for making 6.5 Grendel from 7.62x39; and keeping my 30-06 happy.
I do believe your original question was bulk sizing / application. The alcohol and lanolin is what I use; dump in 1 gallon freezer bag; a few sprays (reuse bag); and then roll around on flat tray to dry. Works fine on turning machine gun brass into usable cases for 7.62 and 5.56. if only I had a faster way to remove the crimps.
-Mac