Are there any videos of the inside of the AMP while annealing? I wonder how "red" the brass gets using it.
I reload some 22-250 for a friend. Even annealing to 750° temiplaq temp, I kept seeing split necks. Bumped up the time on the annealer to get a good glow on them and the splitting has stopped.
I reload some 22-250 for a friend. Even annealing to 750° temiplaq temp, I kept seeing split necks. Bumped up the time on the annealer to get a good glow on them and the splitting has stopped.