First 10 rds were formed using 0.025" jam. Length was 1.541 +/- 0.001" Next 40 rds I used a false shoulder and 0.025"jam. Length was from 1.529" to 1.532". Majority were 1.531". Used 30gr varget, CCI450, 105 AMAX, 0.004" neck tension and blue box lapua brass. Only changes were the barrel was sent to MMI Trutec. Only things I can think of are my chamber was not completely dry and there was imperial sizing wax left on the cases. Any help appreciated