Good day all. First off thanks to all who have been so helpful on this forum. I am new to reloading but wanted to try my hand at casting bullets, so I purchased a Lee mold for 9mm (TC356 124 TC) using reclaimed range lead. Mold seems to work well and got some nice rounds. I plan to PC these rounds and then size them using the Lee resizing kit (.356). I have been looking at videos etc and have a few questions, and I am sure some out there have made and loaded these rounds. I want to size the rounds after PC; any views on this? Also, reloading data seems a little bit variable on this round. I have seen data relating to use of 5.3 grains of Longshot with OAL of 1.05, 3.6 grains of Titegroup with OAL of 1.05 and some other combinations. I have Longshot and Titegroup in stock now. Has anyone out there done anything with these powders and OAL? I figure using range lead should take care of any alloy questions ( I hope anyway). Thanks all.