Case head separation

1. Never use rhe same brass in 2 different rifles.

Very true.


2. The first firing may stretch the brass .010" or more. The 2nd rifle may strerch brass again.

A crush fit, when closing the bolt, is rhe only way to know that the brass has fully expanded to the chamber.

A starting load may make the head to datum measurement shorter. More stretching as the powder charge is increased.
I missed that part about shooting the brass in 2 different rifles! That most likely could be a big problem if the chambers were not the same.
 

Upgrades & Donations

This Forum's expenses are primarily paid by member contributions. You can upgrade your Forum membership in seconds. Gold and Silver members get unlimited FREE classifieds for one year. Gold members can upload custom avatars.


Click Upgrade Membership Button ABOVE to get Gold or Silver Status.

You can also donate any amount, large or small, with the button below. Include your Forum Name in the PayPal Notes field.


To DONATE by CHECK, or make a recurring donation, CLICK HERE to learn how.

Forum statistics

Threads
165,785
Messages
2,203,349
Members
79,110
Latest member
miles813
Back
Top