Dans40X
Welder
bheadboy,
I concur with your philosophy
A 4 or 6 cavity mold actually takes a secondary heat source to keep up to temp.
OP-
Purchase a couple Lee 2 cavity molds as the aluminum pre heats faster than a cast iron mold.
The cost of a Lee 2 cavity mold are equivalent to the cost of other manufacturers handles & are included w/ the Lee molds.
Lee TL(tumble lube) will get you up & running in no time.
I'd suggest sizing all projectiles.
I have a tumble lube recipe that is simple & works well & only takes a few minutes to prepare.
Don't forget the synthetic 2 stroke pre-mix oil as mentioned in the PM's.
I concur with your philosophy
A 4 or 6 cavity mold actually takes a secondary heat source to keep up to temp.
OP-
Purchase a couple Lee 2 cavity molds as the aluminum pre heats faster than a cast iron mold.
The cost of a Lee 2 cavity mold are equivalent to the cost of other manufacturers handles & are included w/ the Lee molds.
Lee TL(tumble lube) will get you up & running in no time.
I'd suggest sizing all projectiles.
I have a tumble lube recipe that is simple & works well & only takes a few minutes to prepare.
Don't forget the synthetic 2 stroke pre-mix oil as mentioned in the PM's.