Seasons Greetings and thank you all for your help to me this year.
I use the K&M kit and have found the following to give splendid consistency in neck wall thickness.
a) Do NOT use a power tool to drive the case on the first cut, do it by hand (if you will pardon the expression)
b) Anneal the case before lathing.
c) Ensure the case is a snug fit on the mandrel
d) Use a small amount of lube on the mandrel AND on the neck of the case.
Comments re the above: -
a) A power tool seems to be OK for fine finishing after the main cut has been made. I.e. where one is only removing the miniscule high spots.
d) I use a very high graphite content grease mixed with STP petrol additive.
I would welcome any advice to improve my understanding.
Cam
I use the K&M kit and have found the following to give splendid consistency in neck wall thickness.
a) Do NOT use a power tool to drive the case on the first cut, do it by hand (if you will pardon the expression)
b) Anneal the case before lathing.
c) Ensure the case is a snug fit on the mandrel
d) Use a small amount of lube on the mandrel AND on the neck of the case.
Comments re the above: -
a) A power tool seems to be OK for fine finishing after the main cut has been made. I.e. where one is only removing the miniscule high spots.
d) I use a very high graphite content grease mixed with STP petrol additive.
I would welcome any advice to improve my understanding.
Cam