First run with my new AMP

I shoot custom KHP 6mm bullets, sort them by OAL .002" variance then trim and point for 600 and 1K competition, all neck tension testing is done after powder charge and seating depth tests.

Maybe save a step Mark and stop measuring by OAL since your trimming them all? Unless you’re trimming to several different OAL’s by batching by similar unmolested OAL’s.

Dave.
 
I test neck tension during load development, I've never tested LO vs HI to see if there's difference on paper, what AMP press tells me how consistent my neck tension is and by sorting I'm not shooting extreme ends of match rounds on score target.
thanks for the info
 
Maybe save a step Mark and stop measuring by OAL since your trimming them all? Unless you’re trimming to several different OAL’s by batching by similar unmolested OAL’s.

Dave.
Dave, there's relatively very little variation in OAL in comparison to other bullets but my OCD would be off the charts if I didn't pre sort :)
 

Upgrades & Donations

This Forum's expenses are primarily paid by member contributions. You can upgrade your Forum membership in seconds. Gold and Silver members get unlimited FREE classifieds for one year. Gold members can upload custom avatars.


Click Upgrade Membership Button ABOVE to get Gold or Silver Status.

You can also donate any amount, large or small, with the button below. Include your Forum Name in the PayPal Notes field.


To DONATE by CHECK, or make a recurring donation, CLICK HERE to learn how.

Forum statistics

Threads
170,037
Messages
2,286,386
Members
82,492
Latest member
Dogdoc
Back
Top