Annealing,
I have read alot of info on this and I do Anneal my brass with Tempilaq 475F about 0.25 below the neck and shoulder junction.
But, I also was reading an article on this site with 650F Tempilaq on the inside of the neck.
What do you guys think the best way to do this? I feel good about using the Tempilaq product and would like to keep using it, just was wondering the best way to go about using it with the best results. Is it bad on brass to anneal every reload or is it best to wait a reload or two?
At first I had trouble getting it off my brass but a little rubbing alcohol will take it right off.
Thanks
Annealing,
I have read alot of info on this and I do Anneal my brass with Tempilaq 475F about 0.25 below the neck and shoulder junction.
But, I also was reading an article on this site with 650F Tempilaq on the inside of the neck.
What do you guys think the best way to do this? I feel good about using the Tempilaq product and would like to keep using it, just was wondering the best way to go about using it with the best results. Is it bad on brass to anneal every reload or is it best to wait a reload or two?
At first I had trouble getting it off my brass but a little rubbing alcohol will take it right off.
Thanks
Annealing,